DISCOUNT / HEYLOVE. Tint base Tinted base FIRE, 15 ml
ATTENTION: there is a minor defect on the bottle! This does not affect the product properties in any way!
Thanks to its dense pigmentation and elasticity, the FIRE tint base creates a perfectly even coverage after just one coat.
Shade: bright red
Collection: MET GALA
Consistency: medium
Stiffness/elasticity: elastic
Acidity: neutral, pH=6.7
Scent: neutral
Pigmentation: dense, covers the free edge
How to use:
-
Thoroughly degrease the nail plate with phBond dehydrator.
- Apply acid-free primer Ultrabond to the nail tip and wait for the liquid to dry completely.
-
Apply a layer of clear Rubber base as a base coat and cure for 30 seconds.
-
Apply one or two coats of Tint base. Cure in UV/LED lamp for 60 seconds.
-
Finish with a layer of top coat.
Volume: 15 ml
Manufacturer: TM "HELLO. by NAILSMADE"
Country: Ukraine
INCI composition: Acrylates Copolymer, HEMA, Trimethylbenzoyl Diphenylphosphine Oxide, Silica Dimethyl Silylate.
- May contain: CI 77891, CI 18965, CI 51319, CI 73915, CI 73360, CI 15510.
Attention! To avoid unwanted polymerization of the material during work, testing, or content shooting, keep the open bottle or brush as far away from daylight as possible (especially from direct sunlight). Also, please note that even in cloudy weather, clouds let through a large amount of ultraviolet radiation, which is enough for the material to start polymerizing.
Note: all documents are in the attached files!
How to prevent bubbles in the material?
Bubbles can appear in any liquid. It does not depend on the formula or ingredients. It depends on the density (viscosity).
It's just a law of physics, nothing else.
For example, in water, bubbles last very briefly and come out on their own.
If we take thicker liquids (honey, thick builder gel, etc.) - in these products, bubbles readily settle in and do not leave them as quickly as water.
So it is with the base. If you work carelessly with the brush, sharply dipping it into the bottle, it involuntarily acts as a blender, mixing the material with air, forming bubbles. This is especially true for materials in bottles with a brush.
Therefore, make CAREFUL, gentle movements with the brush!
Especially when the bottle is new and full.
When we were working on the development of the tint base product, we had a choice of density. We deliberately chose a medium-thick consistency because it has advantages:
- the material does not run or flood;
- contours are sharp without extra effort;
-the master calmly builds the architecture and has time to check it by the highlight;
-there is no need to apply a second coat to refine the architecture or camouflage the free edge.
At our production, we have equipment that prevents the formation of bubbles in the material at all stages – from mixing the pigment to filling into bottles.
We also warn our partners that we are against a store consultant opening a bottle for a customer and showing the material. Because a consultant who is not a nail technician does not understand that bubbles can be created with the brush, even without realizing it.
Not to mention that the bottle necks look unsightly when they are soiled with material to the very top.
If bubbles appear in the material, how to fix it?
Unscrew the bottle cap, but do not pull out the brush.
Place in a warm (but not hot!) place overnight.
Or put the bottle in a plastic bag and immerse in warm water (up to the shoulders).
According to the law of physics, in a warm environment, molecules move faster, and this speeds up the process.
The air will come to the surface, it is lighter than the liquid.