HEYLOVE. Tint base, LACE, 15 ml, tint base
Description
Thanks to its dense pigmentation and elasticity, the tint base LACE creates a perfectly even coating after just the first coat.
Shade: pastel cool pink
Collection: SUNSET
Video: https://www.instagram.com/reel/DObOFRPCGNz/?igsh=MXNocmR1MTVuYjJ6cw==
Consistency: medium
Hardness/elasticity: elastic
Acidity: neutral, pH=6.7
Smell: neutral
Pigmentation: dense, covers the free edge
Application method:
-
Thoroughly degrease the nail plate using a dehydrator phBond.
- Apply an acid-free primer to the nail tip Ultrabond and wait for the liquid to dry completely.
-
Apply a layer of clear base Rubber base as a base coat and cure for 30 seconds.
-
Apply one or two coats of Tint base. Curing time in UV/LED lamp: 60 seconds.
-
Finally, apply a finish coat (top coat).
Volume: 15 ml
Manufacturer: TM "HEYLOVE"
Country: Ukraine
Ingredients (INCI): Polyacrylic Acid, HEMA, Hydroxycyclohexyl Phenyl Ketone, Ethyl Trimethylbenzoyl Phenylphosphinate, Silica. May Contain: Cl 45380, Cl 15850, Cl 77491, CI 15985, CI 77492, Cl 77007, Cl 77510, CI 77742, CI 77289, CI 77499, CI 77891, CI 7700
Warning! To avoid unwanted polymerization of the material during work, testing, or content creation, keep the open bottle or brush as far away from daylight (especially direct sunlight) as possible. Also, please note that even in cloudy weather, clouds transmit a large amount of ultraviolet radiation, which is sufficient for the material to start polymerizing. When painting tips, we recommend keeping the working side of the UV lamp that is turned on away from the master. If you hold the lamp on with the light facing the master, unwanted polymerization of the material on the brushes and necks of open bottles may occur.
Note: all documents are in the attached files!
How to prevent bubbles in the material?Bubbles can appear in any liquid. This does not depend on the formula or ingredients. It depends on density (viscosity).
It's just a law of physics, nothing else.
For example, in water, bubbles last a very short time and come out on their own.
If we take thicker liquids (honey, thick builder gel, etc.) - in these products, bubbles readily settle and do not leave as quickly as water.
The same with base. If you work with the brush carelessly, sharply dipping it into the bottle, it involuntarily acts as a blender, mixing the material with air, creating bubbles. This is especially true for materials in bottles with brushes.
So, make GENTLE, soft brush movements!
Especially when the bottle is new and full.
When we were developing the tint base product, we had a choice of density. We deliberately chose a medium density consistency because it has advantages:
- the material does not run, does not seep;
- contours are clear without extra effort;
- the master can calmly build the architecture and have time to check it by the shine;
- there is no need to apply a second layer to refine the architecture or camouflage the free edge.
At our production facility, there is equipment that prevents the formation of bubbles in the material at all stages – from mixing pigment to pouring into bottles.
We also warn our partners that we are against a store consultant opening a bottle for a client and showing the material. Because a consultant who is not a master does not understand that the brush can create bubbles without even realizing it.
Not to mention that the necks of bottles look unsightly when they are soiled with material to the very top.
If bubbles have appeared in the material, how to fix it?
Unscrew the bottle cap, but do not remove the brush.
Place in a warm (but not hot!) place overnight.
Or put the bottle in a plastic bag and immerse in warm water (up to the shoulders).
According to the law of physics, in a warm environment molecules move faster, and this speeds up the process.
The air will rise to the surface, it is lighter than the liquid.